dc.description.abstractStatement of problem: How variations in salivary chemistry affect the long-term stability of additive manufacturing (AM) and subtractive manufacturing (SM) zirconia is unclear. Purpose: The purpose of this in vitro study was to evaluate the effects of different salivary environments on the color stability, surface roughness, and phase transformation of zirconia fabricated by AM and SM. Material and methods: Disk-shaped specimens (n=160) were fabricated from 4 zirconia materials: 2 AM-AMZ-LI (LithaCon 3Y, produced via lithography-based ceramic manufacturing [LCM]) and AMZ-IN (INNI Cera, produced via digital light processing [DLP])-and 2 SM-SMZ-ST (monolayer Katana ST) and SMZ-ML (multilayer Katana STML). Each material group was divided into 4 subgroups (n=10) based on the aging medium: distilled water (DW), neutral artificial saliva (AS7), acidic artificial saliva (AS4), or enzymatic artificial saliva containing α-amylase (ASE7). Surface roughness (Ra), color change (ΔE₀₀), and phase transformation were assessed. Data were analyzed using a 3-way repeated measures ANOVA with Tukey HSD or Bonferroni post hoc tests (α=.05). Results: Ra was significantly affected by material type, aging condition, and fabrication method (all P≤.001), with AMZ-LI and SMZ-ML maintaining the lowest Ra values (<0.60 µm) after aging. Color stability was similarly influenced (P<.001), with all groups remaining within clinically acceptable limits (ΔE₀₀≤1.8). AMZ-LI (0.60 ±0.08 in DW; max=1.26) and SMZ-ML (0.84 ±0.05 in DW; max=1.20) showed the highest color stability, while SMZ-ST and AMZ-IN had higher ΔE₀₀ in acidic and enzymatic media. Phase transformation was more pronounced in SM groups (P<.05), with SMZ-ML showing the greatest monoclinic increase, and AMZ-LI exhibiting the highest phase stability. Conclusions: Both manufacturing techniques and aging environments significantly affected zirconia's surface, optical, and phase properties. AMZ-LI showed superior resistance to surface and phase degradation, while AMZ-LI and SMZ-ML exhibited the highest optical stability.
dc.identifier.citationSasany R, Uçar SM, Gómez-Polo M, Revilla-León M, Mosaddad SA. Color stability, surface topography, and phase transformation of zirconia fabricated by additive and subtractive manufacturing after exposure to different artificial saliva formulations. J Prosthet Dent. 2026 Jan;135(1):157.e1-157.e10. doi: 10.1016/j.prosdent.2025.09.021. Epub 2025 Oct 1. PMID: 41038731.
dc.identifier.doi10.1016/j.prosdent.2025.09.021
dc.identifier.issn0022-3913
dc.identifier.issn1097-6841
dc.identifier.issue1
dc.identifier.pmid41038731
dc.identifier.urihttps://hdl.handle.net/11363/11941
dc.identifier.volume135
dc.indekslendigikaynakPubMed
dc.language.isoen
dc.publisherMosby
dc.relation.ispartofThe Journal of Prosthetic Dentistry
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/openAccess
dc.titleColor stability, surface topography, and phase transformation of zirconia fabricated by additive and subtractive manufacturing after exposure to different artificial saliva formulations
dc.typeArticle

Dosyalar

Orijinal paket

Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
Makale / Article.pdf
Boyut:
4.48 MB
Biçim:
Adobe Portable Document Format

Lisans paketi

Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
license.txt
Boyut:
1.17 KB
Biçim:
Item-specific license agreed upon to submission
Açıklama: