<link rel="stylesheet" href="styles.f3b1fba60ec7970c.css">

Yayın:
Durability of Alkali-Activated Concretes Under 5% Sulfuric Acid Environment

dc.authorid0000-0003-4003-1672
dc.authorid0000-0001-9092-8088
dc.contributor.authorKarabaş, Celal
dc.contributor.authorNiş, Anıl
dc.contributor.institutionauthorNİŞ, ANIL
dc.date.accessioned2026-02-02T10:22:47Z
dc.date.issued2025
dc.departmentMühendislik ve Mimarlık Fakültesi
dc.description.abstractThe investigation focused on the resistance to 5% sulfuric acid degradation of the alkali-activated concretes (AAC). The AAC was manufactured using a blended binder of 50% slag and 50% F-type fly ash. The AAC was activated using a blend of 14 M sodium hydroxide and sodium silicate, with a hydroxide-to-silicate ratio of 1/2,5. Six AAC were produced against a 5% sulfuric acid environment, varying the binder amounts (400–500–600 kg/m3 ) and activator-binder (A/B) ratios (0,45–0,55). The chemical resistance of AAC was evaluated by visual appearance, variation in weight and compressive strengths. The findings pointed out that more gypsum and higher weight gain were obtained on the AAC specimens having 600 kg/m3 binder content. There is no or negligible influence of A/B ratio was found on the visual appearance and weight variation after acid attack. The results revealed that the highest durability was achieved with the maximum binder content of 600 kg/m3 combined with the 0,45 A/B ratio, while the lowest resistance was achieved with the minimum binder content of 400 kg/m3 and 0,55 A/B ratio. The additional water content of 7,5% by binder weight should be reduced to achieve higher mechanical strength for the AAC, especially for high-binder mixes (>400 kg/m3 ).
dc.identifier.doi10.29187/2458-973X.1203
dc.identifier.endpage531
dc.identifier.issn2458-973X
dc.identifier.issue4
dc.identifier.scopus2-s2.0-105026258342
dc.identifier.scopusqualityQ3
dc.identifier.startpage522
dc.identifier.urihttps://hdl.handle.net/11363/11094
dc.identifier.volume10
dc.institutionauthorKarabaş, Celal
dc.institutionauthorNiş, Anıl
dc.institutionauthoridhttps://orcid.org/0000-0003-4003-1672
dc.institutionauthoridhttps://orcid.org/0000-0001-9092-8088
dc.language.isoen
dc.publisherYildiz Technical University
dc.relation.ispartofJournal of Sustainable Construction Materials and Technologies
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectAlkali activated concrete (AAC)
dc.subjectSulfuric acid attack
dc.subjectVisual inspection
dc.subjectWeight change
dc.subjectCompressive strength
dc.titleDurability of Alkali-Activated Concretes Under 5% Sulfuric Acid Environment
dc.typeArticle
dspace.entity.typePublication
dspace.relatedentity.typePerson
local.indexed.atScopus
local.indexed.atTRDizin
person.identifier.orcid0000-0001-9092-8088

Dosyalar

Orijinal paket

Şimdi gösterimde1 - 1 of 1
Yükleniyor...
Küçük Resim
Adı:
Makale / Article.pdf
Boyut:
24,82 MB
Format:
Adobe Portable Document Format

Lisans paketi

Şimdi gösterimde1 - 1 of 1
Yükleniyor...
Küçük Resim
Adı:
license.txt
Boyut:
1,17 KB
Format:
Item-specific license agreed upon to submission
Description: